Cable Paper

Description:
Cable Paper is made of two layers of Aramid paper with one layer of Polyimide film, with good dielectric properties, high heat resistance and mechanical strength, and suitable for electric motors as slot, phase, turn-to-turn, liner insulation in H-class Motor.

Main Specification:

Properties

Values

Structure

212

222

232

242

252

262

2 7.5 2

3 7.5 3

Normal thickness(mm)

0.13

0.15

0.18

0.20

0.24

0.25

0.30

0.30

Thickness Tolerance(mm)

+/-10%

Specific Weight(g/m2)

134

169

205

240

280

315

370

390

Specific Weight tolerance

+/-10%

Tensile Strength (N/cm) unfold ≥

MD

95

150

140

170

190

195

260

280

TD

65

85

100

110

130

160

215

240

Breakdown Voltage(KV)(Unfold) ≥

5.0

8.0

10

12

14

15

18

18

Bonding Strength at 25c.

No Delamination

Bonding Strength at 200c 10min

No Delamination, No Blister, No Adhesive Flow

Testing Method

GB/T 5591.2-2002 or IEC 60626-2:1995